Altermix DTDM-80GE
80% 4,4′-Dithiodimorpholine (Sulfur donor) pre-dispersed masterbatch
Typical Properties
Items | Typical values |
Appearance | Gray-white granule |
Density | 1.10g/cm3 |
Mooney viscosity ML (1+4) @ 50°C |
42 |
Product features and dosage
AlterMix DTDM-80GE is suitable for both natural rubber and synthetic rubber. The rubber used in this product has no the phenomenon such as blooming, pollution, discoloration, etc., and has a good dispersibility.
The vulcanized rubber obtained from EV and SEV curing system with DTDM-80GE has a good heat resistance and aging resistance, and the compression set is lower.
AlterMix DTDM 80GE can decompose active sulfur at the vulcanization temperature. The effective sulfur content is 27%,it is safe to operate. The vulcanization is slow when used DTDM alone, however the speed will be improved when combined with thiazoles, thiurams and dithiocarbamates.
AlterMix DTDM-80GE is especially suitable for IIR, it is mainly used in the manufacture of tires, inner tubes of IIR, tapes and heat resistant rubbers.
Dosage:0.5-2.5 phr.
Packaging and storage
25KG/carton packaging,
Product limited use date: 3 years
Store in a dry environment at room temperature, avoid direct sunlight and keep away from heat sources.