Home / Sulfur donor / Altermix DTDM-80GE

Altermix DTDM-80GE

 

Altermix DTDM-80GE

80% 4,4′-Dithiodimorpholine (Sulfur donor) pre-dispersed masterbatch

 

Typical Properties

 

Items Typical values
Appearance Gray-white granule
Density 1.10g/cm3
Mooney viscosity ML (1+4) @ 50°C  

42

 

 

Product features and dosage

AlterMix DTDM-80GE is suitable for both natural rubber and synthetic rubber. The rubber used in this product has no the phenomenon such as blooming, pollution, discoloration, etc., and has a good dispersibility.

The vulcanized rubber obtained from EV and SEV curing system with DTDM-80GE has a good heat resistance and aging resistance, and the compression set is lower.

AlterMix DTDM 80GE can decompose active sulfur at the vulcanization temperature. The effective sulfur content is 27%,it is safe to operate. The vulcanization is slow when used DTDM alone, however the speed will be improved when combined with thiazoles, thiurams and dithiocarbamates.

AlterMix DTDM-80GE is especially suitable for IIR, it is mainly used in the manufacture of tires, inner tubes of IIR, tapes and heat resistant rubbers.

Dosage:0.5-2.5 phr.

 

Packaging and storage

25KG/carton packaging,

Product limited use date: 3 years

Store in a dry environment at room temperature, avoid direct sunlight and keep away from heat sources.

 